The comparative characteristic values for tensile strength RIm andRIp0.2 yield strength to tensile test determined by the indentation method lie within a statistically determined confidence range . You will find a current overview of this under the heading Materials.

Tensile test and indentation methods show systematic errors. Material-specific material cards can be created to reduce the deviation. The basis for this is provided by tensile specimens and the associated stress-strain diagrams. Comparison measurements are used to calibrate the results from the indentation method to the results of the tensile test.

We will be happy to send you documentation on this on request.